TECHNET Archives

February 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 26 Feb 2008 11:43:09 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
From:
Joyce Koo <[log in to unmask]>
content-transfer-encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (24 lines)
Does any of old chaps still got this?  Thanks.
                         jk
Optimization of solder paste printability with laser inspectiontechnique
Okura, T.; Kanai, M.; Ogata, S.; Takei, T.; Takakusagi, H.
Electronics Manufacturing Technology Symposium, 1995. apos;Manufacturing Technologies - Present and Futureapos;, Seventeenth IEEE/CPMT International
Volume , Issue , 2-4 Oct 1995 Page(s):361 - 365
Digital Object Identifier   10.1109/IEMT.1995.526187
Summary:This paper describes an evaluation technique for solder paste printability using a solder paste inspection system and optimization of printing parameters. In a Surface Mount Assembly (SMA), it is very important to evaluate printability of solder paste precisely, because printability of solder paste directly influences reflow soldering quality. We established quite reliable inspection criteria for print quantity of solder paste. So it was found that about 90% of reflow soldering defects could be reduced by prevention of printing defects. Furthermore, since package types have been varied in a SMA, high soldering quality demands stable printability for all patterns. This paper presents a printability evaluation adopted procedure based on the quality engineering (TAGUCHI method). As a result of optimizing squeegee shape and printer condition by this evaluation method, printability was improved better than 20% in the production process. And optimization of solder paste and stencil added to printer condition resulted in good printability for 0.3 mm pitch patterns on the optimum condition



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2