TECHNET Archives

February 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 22 Feb 2008 16:50:10 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (62 lines)
Hi Werner! Ok, so you don't want to read the whole web site! : - ) 

Here is a more specific link:

http://acqp2.nasa.gov/LFS%20Reliability/Rockwell%20Collins%20Inc%20JCAA%20JGPP%20Final%20Report%20neg55C%20to%20pos125C%20testing%20Rev%20B.pdf

The shrinkage void data is in the Thermal Cycle individual report (see 
figure 45, page 33) on shrinkage voids. We ran thermal cycle testing -55C 
to +125C for 4700+ cycles per IPC-9701 and did not find an occurrence were 
a shrinkage void caused a failure or acted as a stress riser.

Dave



[log in to unmask] 
02/22/2008 04:37 PM

To
[log in to unmask], [log in to unmask]
cc

Subject
Re: [TN] Shrink hole voids






Hi Dave & All,
http://acqp2.nasa.gov/LFS%20Reliability/JTR%20Executive%20Summary%20Draft%20July-14-2006.pdf
JCAA/JG-PP Lead-Free solder Project, Joint Test Report, Draft July 14, 
2006 only makes a one-sentance statement that "Solder Joint Shrinkage 
Voids and Fillet Lifting: No thermal cycle failures were observed due to 
the presence of solder joint shrinkage voids or fillet lifting phenomena."
I certainly would not draw any conclusions from this.
Coyle's paper deals with gaseous voids, not shrinkage voids.




Werner



**************
Ideas to please picky eaters. Watch video on AOL Living.
(
http://living.aol.com/video/how-to-please-your-picky-eater/rachel-campos-duffy/2050827?NCID=aolcmp00300000002598
)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2