Hi David,
Think of rivets on a plane or ship. They are there to prevent a crack
from propagating. A hole (or void) will do the same trick. It does not
create a stress concentration (particularly in a ductile material like
solder) and therefore it can stop a crack ("swallowing" it). You can
take a look at the basics of Fracture Mechanics if you want to.
Regards,
Vladimir
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
Sent: Friday, February 22, 2008 1:29 PM
To: [log in to unmask]
Subject: [TN] Shrink hole voids
Hello TechNet Gurus,
I read an article that say that a shrink hole void (hot tear or sink
hole)
is not a crack, does not impact reliability, does not continue to grow
under
thermo-mechanical stresses.
This seems to go against my common sense and would venture to say adds
to
solder creep fatigue.
Would anyone like to comment on my comment and/or offer a link to where
I
can find more information?
I am a poor country and your two cents goes a loooooong way.
As always, thank you in advance.
Thank you,
David Tremmel
Value Recovery
847 858-5540 - Cell
847 557-9574 - Office
847 557-9573 - Fax
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|