Before you dig too deep in your pocket, you should have someone try an
FTIR scan. Take a quick look at:
http://www.ipc.org/4.0_Knowledge/4.1_Standards/test/2.3.39C.pdf
Nice thing about this technique is the solvent it recommends.
Acetonitrile will dissolve about any organic residue out there and it's
easy to evaporate for analysis. A good FTIR data base should at least
get you close to the general class of chemical you're dealing with and
at minimum provide you with a direction.
A complicating issue with any analysis might be that:
#1 - you are dealing with multiple chemical compounds in the residue.
#2- this is not a residue at all, but an attack/discoloration of the
surface.
Rich K / GTS
847-621-7310
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg
Sent: Thursday, February 21, 2008 3:53 PM
To: [log in to unmask]
Subject: [TN] Residues
We are having an issues with printed circuit boards showing residues,
that become more prevalent after heating cycles. It leaves a shiny /
oily
looking film that is somewhat splotchy. Sorry for all these technical
terms.
I'm suspecting undercured epoxy, and I am currently looking to send
some out for chemical analysis. I have one lab quoting IC, and another's
website also recommends FT-IR. The supplier performed a ROSE test
and says there is no ionic contamination. The biggest problem we are
having is with conformal coating adherance. Due to certain components
on the one board that gives us trouble we aren't able to run it trhough
our aqueous wash cycle.
Is Ion Chromatography the right test? Any other suggestions?
Thanks,
Blair
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|