Secondary Ion Mass Spectrometry (SIMS) and/or X-ray Photoelectron
Spectroscopy can almost certainly tell you the chemistry of a thin layer
such as the one you describe. Probably Time-of-Flight SIMS would be the
most sensitive and best able to give you a definitive answer.
You could try calling Evans Analytical Group (eaglabs.com) and discuss with
one of their TOF-SIMS analysts.
Noel
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
Sent: Thursday, February 21, 2008 1:36 PM
To: [log in to unmask]
Subject: Re: [TN] Residues
Blair: My suspicion is that IC will tell you essentially nothing. From the
sound of your highly technical description, I would bet the residue is
largely organic, and most organics do not ionize, so IC would tell you
little.
It MIGHT be flux residue, what sort are they using?
Would recommend trying to dissolve the residue in a solvent, and send out
for GC-Mass spec.
Even an elemental analysis would give you a direction to move in.
Rudy Sedlak
RD Chemical Company
Blair Hogg <[log in to unmask]> wrote: We are having an issues with
printed circuit boards showing residues,
that become more prevalent after heating cycles. It leaves a shiny / oily
looking film that is somewhat splotchy. Sorry for all these technical
terms.
I'm suspecting undercured epoxy, and I am currently looking to send
some out for chemical analysis. I have one lab quoting IC, and another's
website also recommends FT-IR. The supplier performed a ROSE test
and says there is no ionic contamination. The biggest problem we are
having is with conformal coating adherance. Due to certain components
on the one board that gives us trouble we aren't able to run it trhough
our aqueous wash cycle.
Is Ion Chromatography the right test? Any other suggestions?
Thanks,
Blair
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Looking for last minute shopping deals? Find them fast with Yahoo! Search.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|