Had the same problem with an edge connector oozing contaminants when I
checked it by omegameter in as received condition. Thinking about degolding
of the pins on the soldering area and bad cleaning afterwards. Could it be?
Gaby
----- Original Message -----
From: "Graham Collins" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, February 19, 2008 7:35 PM
Subject: [TN] cleanliness testing
Hello TechNet
I'm in a debate with a supplier about the incoming cleanliness of one of
their parts, they claim it's squeaky clean and I claim it's as salty as a
bag of salt & vinegar potato chips. Obviously we are both exaggerating, but
one of us has a good claim.
They are fending me off with resistivity measurements made per the manual
test method IPC-TM-650 2.3.25 - which works in that I don't know how to
convert it to the "ug NaCl/in2" equivalent units I'm used to. Is there a
valid conversion?
Sir Doug of Dew, if you reply please do NOT say it depends...
regards,
Graham Collins
Halifax Production Engineering
L-3 communications Electronic Systems
(902) 873-2000 ext. 6215
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|