IPC-600-6012 Archives

February 2008

IPC-600-6012@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
IPC-600-6012<[log in to unmask]>
Subject:
From:
John Perry <[log in to unmask]>
Date:
Mon, 4 Feb 2008 14:52:57 -0600
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"(Combined Forum of D-33a and 7-31a Subcommittees)" <[log in to unmask]>
Parts/Attachments:
text/plain (48 lines)
Colleagues,

 

Our IPC-6012B specification provides for bare copper as a final finish
in Table 3-2, Final Finish, Surface Plating and Coating Thickness
Requirements.

 

The task group is evaluating whether or not this should be removed from
Table 3-2 in the future IPC-6012 Revision C.  Among the concerns with
bare copper are instances of single-sided via protection that provides
for entrapment of chemistries that attack the bare copper in the hole
wall.

 

If there are those of you out there who use bare copper as a surface
finish, could you provide feedback to IPC as to how it is used in your
applications?

 

Thanks in advance,

 

John Perry

Technical Project Manager

IPC

3000 Lakeside Drive # 309S

Bannockburn, IL 60015

[log in to unmask]

1-847-597-2818 (P)

1-847-615-7105 (F)

1-847-615-7100 (Main)

 

ATOM RSS1 RSS2