Yesskij, seems to be, but there is one article from 2007 also. The concept may be further improved today, see below:
http://www.techbriefs.com/index.php?option=com_staticxt&staticfile=Briefs/Mar02/LEW16890.html
There are better descriptions, butI can't find them.
Anyway, carbon reinforcement is of interest. If you do searching in Germany, France, Japan etc, I'm sure you will find even more advanced concepts with carbon stiffener. Sorry enough, there are just a couple of TN persons that represent those countries, Mike Fenner for England...and Brian Ellis for the rest of Europe.
If there is a warpage wave soldering problem at Leadfree temp, you can always go back to 'pallets', which were frequently used as early as 1960, if I'm right.
http://circuitsassembly.com/cms/content/view/3420/95/
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: den 9 januari 2008 12:59
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] Warpage of components
Inge,
All your keywords match this short article:
http://findarticles.com/p/articles/mi_qa3957/is_200203/ai_n9041332
But again, this article is nearly 6 years old.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Wednesday, January 09, 2008 3:42 AM
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] Warpage of components
Hi yaself!
Njetskij, sorry, what I aimed at is a very recent invention, Stablcor has existed for a decade.
If there is a NASA guy among the TNetters, he may find by searching at 'carbon cloth PWB' or 'carbon reinforced boards' or something like.
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: den 8 januari 2008 23:24
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] Warpage of components
Hi Inge!
I bet you're referring to Stablcor...
http://www.stablcor.com/
At a past life the company that I worked for looked into the material to help ruggedize a Single-board Computer. Didn't really get to play around with it though. Couldn't get all involved to buy-off using the material because it was so new.
But I must say, it looks pretty interesting! Wish I could have got some experience with it.
Steve Gregory
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Tuesday, January 08, 2008 3:16 PM
To: [log in to unmask]
Subject: [TN] SV: [TN] Warpage of components
If someone has a 'warpage' problem, there is a way to design boards that are less apt to bending. NASA are working with new ideas, and Glenn Research Center together with Applied Materials, are making the new hardware. This is a carbon cloth, that is integrated with the FR4. The benefit is better cooling, better electrical performance and much stiffer board, the later means little or no warpage. I've seen these boards, but can't find the source at the moment. I'm sure someone on TN have more to show us here.
If there are patent matters that hinder you for using the concept, I don't know.
If I find more on this theme, I'll be back.
/Inge
-----Ursprungligt meddelande-----
Från: Hfjord [mailto:[log in to unmask]]
Skickat: den 8 januari 2008 16:56
Till: 'TechNet E-Mail Forum'; [log in to unmask]
Ämne: SV: [TN] Warpage of components
I promised a simple warpage calculation formula, if not too many, I'll send offline...
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Werner Engelmaier /*
Skickat: den 8 januari 2008 14:15
Till: [log in to unmask]
Ämne: Re: [TN] Warpage of components
HI Ingemar,
Well said.
A warpage criterion for components would have to be based on a total out-of-plane measurement at soldering temperatures. This non-coplanarity measure would have to be about the thickness of the solder paste layer to avoid solder opens, and it would have to be based on the total final solder joint thickness to avoid solder joint cracking due to warpage tensile loads on cooling from reflow.
Werner
**************
Start the year off right. Easy ways to stay in shape.
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|