TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Anat Douek <[log in to unmask]>
Date:
Thu, 31 Jan 2008 14:20:34 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (167 lines)
Choose ONLY the gold over nickel plating under those circumstances, 
otherwise you will make yourself a stick for own back for a few cents. 
False economy.

Brian

Anat Douek wrote:
> It is OSP Panel feedthru connector made by MAACOM.
> Maacom has two options of the housing bushing plating :
> 1. stainless steel type 303 passivated per ASTM A 380
> 2.  stainless steel type 303 with gold over nickel plating.
> 
> Since option 1 is chipper we would like to purchase it, but our customer,
> who supposed  to connect  his mating connector, has  connector made of
> stainless steel type 303 with gold over nickel plating.
> I hope it is clear now.
> Thank you in advance.
> Anat
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
> Sent: Thursday, January 31, 2008 1:37 PM
> To: [log in to unmask]
> Subject: Re: [TN] galvanic compatibility
> 
> this gives a different image. Seems like risk for galvanic currents.
> However, I'm still confused. 
> 
> A  connector with passivated stainless steel 303?? What kind? 
> 
> And the gold plated connector, what's the body made of? Steel 303? 
> 
> Are you talking coaxial SMT SMA connectors or like? If that is the case, you
> must have steel-to-steel or gold-to-gold. 
> 
> /Inge
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Anat Douek
> Sent: den 31 januari 2008 10:45
> To: [log in to unmask]
> Subject: Re: [TN] galvanic compatibility
> 
> 
> Thank you for your response.
> It is not double plating. I have one connector  with passivated stainless
> steel 303 and the mating connector is gold plating.
> The question is if it  can be joined together,  in high humidity level,
> without creation of corrosion Anat
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
> Sent: Thursday, January 31, 2008 10:29 AM
> To: [log in to unmask]
> Subject: Re: [TN] galvanic compatibility
> 
> Anat,
> 
> why gold on passivated steel? Cosmetic aspect? 
> Well, if it's a must, gold over steel is possible.
> There are lots of products with that finish, e.g. wrist watches.
> 
> Passivation of steel is for protection against corrosion Gold plating is
> also for protection against corrosion.
> So, you want a double corrosion protection?
> 
> Gold is not corrosive in itself and works as a corrosion protection if the
> gold is thick and free from pores. If too thin gold is used, corrosion can
> start through pores in the gold plating. 
> 
> So, if you happen to have minor contaminations in the steel AND a porous
> gold plating, there is a risk of pore corrosion. The steel surface roughness
> is also of importance.
> 
> As always, there are some 'it depends'. If you describe the part to be
> plated, TN may give you a more precise answer.
> 
> 
> Inge 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Anat Douek
> Sent: den 30 januari 2008 14:37
> To: [log in to unmask]
> Subject: [TN] galvanic compatibility
> 
> 
> Hi,
> Is passivated stainless steel 303 can be joined to gold plating,  in high
> humidity level,  without creation of corrosion ?
>  
> Regards,
> Anat
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please visit
> IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please visit
> IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please visit
> IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit IPC web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2