TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 24 Jan 2008 07:48:05 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, al shirazi <[log in to unmask]>
Subject:
From:
al shirazi <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (49 lines)
Hi Werner,

Sorry that was the subject of the other e-mail that I just used its block to send my e-mail.I guess I missed it!Sorry for the confusion!

In fact I am investigating the finite element models to include the intermetallic layer, to me should have a significant impact on thermo-mechanical durability of the SAC joint. The change of the solder composition near the intermetallic layer due to metalization. 
Please correct if I am wrong!

Al

Werner Engelmaier /* <[log in to unmask]> wrote: Hi Al, 
Why do you subject this "Coffin-Manson"?
Coffin-Manson does not work for solder.



Werner



**************
Start the year off right.  Easy ways to stay in shape.
     
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


       
---------------------------------
Looking for last minute shopping deals?  Find them fast with Yahoo! Search.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2