TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 18 Jan 2008 14:41:52 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (182 lines)
An Englishmans "California moments".

So in 2001 I was living in Corona out in the desert near LA. In January of
that year I jumped in the car - started the engine, turned on the wipers to
clear the condensation and found that the windshield wiper motor had packed
up.

I went back into the house and told my wife who had been living for years in
Colorado, who burst out laughing and suggested I get a can of de-icer, or
use some water to melt the ice that had frozen them to the
windshield.....................

In February that year I was doing some work on anisotropic adhesive bonding
and recounted this tale to the 3M rep who was helping me with the project.
He laughed and said "If you think that's funny, I have a garage full of 3M
seasonal marketing giveaways that I can't even give away in California - 20
boxes of Windshield Ice scrapers with the 3M logo on
them.......................

Have a great weekend everyone.....8-)

 
 
John Burke
 
(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Friday, January 18, 2008 2:20 PM
To: [log in to unmask]
Subject: Re: [TN] Solderability of Tin-Gold Intermetallic NTC

Ahhh Ontario, the California of Canada................

Doug Pauls




Bev Christian <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
01/18/2008 04:03 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bev Christian <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Solderability of Tin-Gold Intermetallic NTC






Now Genny, we mustn't exaggerate. It is only -23.5C most of the time and
we get 7 hours every other Wednesday.

Seriously most of southern Ontario is at the same latitude as southern
Oregon/northern California and although it is not as warm as those
states, it is certainly comparable to a lot of the New England, Mid
Atlantic and Midwestern lake states.

However, I lived two years in Edmonton, Alberta (1980-82, the most
northernly, large city (>1M) in North America) and in the winter of
81-82 we had six weeks when the highest it got was -25C and it was -45C
at night (excluding wind chill).  On top of that this post doc had no
car, my wife and I had two little kids and there was a bus strike at the
same time. Getting groceries was "interesting". Oh, and the sun came up
after 9 AM and set by about 4 PM.  Yuck.  I did like the sunny, open
skies and the stuff you hear about a dry cold compared to -4C in Seattle
or Vancouver, British Columbia is actually true.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Friday, January 18, 2008 4:41 PM
To: [log in to unmask]
Subject: Re: [TN] Solderability of Tin-Gold Intermetallic NTC

!!!   Shhhhh don't give away our secrets.
How else do you think we deal with months of -25C or colder weather and
only 6 hours of sunlight a day...
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: January 18, 2008 3:30 PM
To: [log in to unmask]
Subject: Re: [TN] Solderability of Tin-Gold Intermetallic NTC

Usually all of Canada is lumped into one state...

Yes, an altered state.
Dewey

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 
information. Any use of this information by anyone other than the intended 
recipient is prohibited. If you have received this transmission in error, 
please immediately reply to the sender and delete this information from 
your system. Use, dissemination, distribution, or reproduction of this 
transmission by unintended recipients is not authorized and may be 
unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2