TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 3 Jan 2008 15:13:29 -0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Colin McVean <[log in to unmask]>
Subject:
From:
Colin McVean <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (217 lines)
I also found this interesting article about implants

http://www.mdtmag.com/scripts/ShowPR.asp?PUBCODE=046&ACCT=0000100&ISSUE=
0510&RELTYPE=PR&PRODCODE=0000&PRODLETT=B



Colin W.T. McVean M.Inst.C.T                                
Production Manager
 
 
Artetch Circuits Ltd  (www.artetch.co.uk)
Direct Dial      01903 712926
Switch Board  01903 725365
Skype: colin.artetch                                           
40th Anniversary 1967 - 2007
Before printing , please think about the Environment       

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Colin McVean
Sent: 03 January 2008 14:51
To: [log in to unmask]
Subject: Re: [TN] liquid imageable soldmask

Then you are going to be looking at the likes of flexible Kapton
coverlayer type materials rather than a solder mask. I think Dupont have
a specific medical grade version

Colin W.T. McVean M.Inst.C.T                                
Production Manager
 
 
Artetch Circuits Ltd  (www.artetch.co.uk)
Direct Dial      01903 712926
Switch Board  01903 725365
Skype: colin.artetch                                           
40th Anniversary 1967 - 2007
Before printing , please think about the Environment       
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Seymour
Sent: 03 January 2008 14:37
To: [log in to unmask]
Subject: Re: [TN] liquid imageable soldmask

This device would be implanted below the skin.

Thanks
dave


Douglas O. Pauls wrote:

>Well now Dave, it depends.
>
>What do you mean by medical application?  Is this being inserted inside

>someone?  An electrical device exposed to bodily fluids?  High
reliability 
>or life critical function?
>
>I would probably start with Taiyo PSR-4000.  Works pretty good on our
high 
>reliability stuff.
>
>Doug Pauls
>
>
>
>
>Dave Seymour <[log in to unmask]> 
>Sent by: TechNet <[log in to unmask]>
>01/02/2008 03:12 PM
>Please respond to
>TechNet E-Mail Forum <[log in to unmask]>; Please respond to
>Dave Seymour <[log in to unmask]>
>
>
>To
>[log in to unmask]
>cc
>
>Subject
>[TN] liquid imageable soldmask
>
>
>
>
>
>
>Does anyone have any recommendations for a photo imageable solder
>mask that can be used in a medical application? 
>
>Thanks
>dave
>
>
>Dave Seymour, CID+
>Catapult Communications Inc.
>800 Perimeter Park Dr, Suite A
>Morrisville, NC 27560
>
>Direct: (919)653-4249
>Main: (919)653-4180
>Fax: (919)653-4297
>
>[log in to unmask]
>
>
>
>
>
>
>
>***********************************************************************
**********************************
>"This e-mail (and any attachments) is confidential and privileged 
>information of Catapult Communications"
>***********************************************************************
**********************************
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to 
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to 
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
http://listserv.ipc.org/archives
>Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
>for additional information, or contact Keach Sasamori at [log in to unmask]
or 
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
http://listserv.ipc.org/archives
>Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
>-----------------------------------------------------
>
>  
>

-- 
Dave Seymour, CID+
Catapult Communications Inc.
800 Perimeter Park Dr, Suite A
Morrisville, NC 27560

Direct: (919)653-4249
Main: (919)653-4180
Fax: (919)653-4297

[log in to unmask]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2