Just stick with what you're comfortable with.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, January 11, 2008 1:41 PM
To: [log in to unmask]
Subject: Re: [TN] Bottom side SMT adhesives
Hi Larry!
Since I couldn't think of a good retort, I guess I have to be the one
with a serious response... ;^)
I use EpiBond 7275 and have not had any issues.
I like the Epibond for a few more reasons than just the way it performs;
1), It's shelf life is longer than any of the Loctite products, 2), It's
easier to get in the small quantities that we use, and 3), The Leadtime
to get it is nowhere near what Loctite is...
Steve Gregory
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Davis, Larry
Sent: Friday, January 11, 2008 2:32 PM
To: [log in to unmask]
Subject: Re: [TN] Bottom side SMT adhesives
I should've known better than to ask on a Friday...
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Friday, January 11, 2008 1:29 PM
To: [log in to unmask]
Subject: Re: [TN] Bottom side SMT adhesives
Well, it was the least I could since it appears the Aurora Borealis
dipped downed on Cedar Rapids and evoked a startling epiphany of cosmic
clarity from the two local legends/icons today on Technet. I figure
someone with weighted grammar had to balance the scale.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Friday, January 11, 2008 12:20 PM
To: [log in to unmask]
Subject: Re: [TN] Bottom side SMT adhesives
Glad to see you are applying Dewey diligence to the humour
issues.....8-)
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Friday, January 11, 2008 9:56 AM
To: [log in to unmask]
Subject: Re: [TN] Bottom side SMT adhesives
Sorry, Sir we only due levity on Friday. Levitate is on Monday.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Davis, Larry
Sent: Friday, January 11, 2008 10:38 AM
To: [log in to unmask]
Subject: [TN] Bottom side SMT adhesives
Happy Friday Everyone!
We are currently stencil printing Loctite 3612 for our bottom side SMT
parts. We have trouble getting larger parts (SOL's, tantalums, etc) to
stay attached consistently. I'm just wondering what products others are
using for this process and if anyone has had the same issue.
Thanks and have a great weekend!
Larry
This message (including any attachments) contains confidential and/or
proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on the
contents of this information is strictly prohibited and may constitute a
violation of law. If you are not the intended recipient, please notify
the sender immediately by responding to this e-mail, and delete the
message from your system. If you have any questions about this e-mail
please notify the sender immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential and/or
proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on the
contents of this information is strictly prohibited and may constitute a
violation of law. If you are not the intended recipient, please notify
the sender immediately by responding to this e-mail, and delete the
message from your system. If you have any questions about this e-mail
please notify the sender immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|