Two other things to watch if using natural latex masking compound with
conformal coating.
Do not try and cure latex above 50C as you will end up with a sticky mess on
the board, that is hard to remove.
If the conformal coating you are using is a thermal cross linking silicone,
the masking material could inhibit curing of the coating, no matter how much
heat you put in.
Best Regards
David Greenman
Managing Director
HumiSeal Europe Ltd
A British Manufacturer : Part of Chase Specialty Coatings
[log in to unmask]
www.humiseal.eu
www.chasespecialtycoatings.com
==========================================
HumiSeal Europe Ltd
Registered in England & Wales No : 1480710
Registered Office : Albany Park, Frimley Road, Camberley, Surrey, GU16 7PH
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne
Sent: 09 January 2008 23:24
To: [log in to unmask]
Subject: Re: [TN] Coating
We have lots of experience with the peelable masks. They are pretty
inert and leave no detectable residue provided they peel off cleanly.
There are two significant problems:
1. In order to peel off cleanly, they need to be put on pretty
thick--like 0.5mm thick. At this thickness, your resolution is not so
good, and it interferes with the solder stencil, so you need a stencil
cutout over that area and need to work at it to get decent
printing--maybe even hand squeegee the paste in.
2. If you get them hot for too long, they embrittle. Then you are in
for some serious problems getting them off cleanly. The thinner you put
them on, the less temperature/time they need to get this way.
We've also used water soluble. These work pretty good unless you are
trying to protect gold wirebond pads: The flux chemistry goes through
them pretty easily, but the solder won't wet the area. I don't have
data for contamination levels after removal, but we didn't have a
problem during the time we used them. Of course, these won't survive a
cleaning process.
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Wednesday, January 09, 2008 5:41 PM
To: [log in to unmask]
Subject: Re: [TN] Coating
Yannick,
We don't do that here, but when I was at Nortel we did quite bit. You
need to make sure the temporary solder mask is not going to cause
corrosion, especially if it is hard to remove and will be leaving bits
and pieces on your boards!
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Yannick Brisson
Sent: Wednesday, January 09, 2008 4:57 PM
To: [log in to unmask]
Subject: [TN] Coating
Hi,
I'm wondering what you guys do for coating a PCB with area to mask?
do you use something special, Do you do your jigg yourself, or do you
send it to some other specialize in it?
Thank you
Yannick
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|