Peer, microwave boards?
You can use conventional belt ovens, batch ovens or VP ovens, just a
question of temp curve. Ericsson have soldered some 2,000,000 brass backed
boards with belt oven. You have to create your own window, copying other's
won't work, unless the mass is same as well as geometry and component
selection. Speak to your oven manufacturer, he may have thumb rules to start
with. The trick is to increase the preheat time without affecting the flux,
and get a rapid cool down, the middle of the curve should be same as for
ordinary boards. All depending on the metal mass, which one you don't
mention. Myself, I would use VP, no problem with IR absorption, flux
charring and a lot of zone adjustments. Just to dive...(not the full
truth..)
By the way, is someone following/using this one microwave board spec from
Year 2006 or is there a fresher one?
http://av.rds.yahoo.com/_ylt=A9ibyKXB8ntHVP8AujwDRaMX;_ylu=X3oDMTBvdmM3bGlxB
HBndANhdl93ZWJfcmVzdWx0BHNlYwNzcg--/SIG=12fjc87me/EXP=1199391809/**http://me
mbers.ipc.org/committee/drafts/D-22_d_6018BWD1.pdf
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För P. Langeveld
Skickat: den 2 januari 2008 16:58
Till: [log in to unmask]
Ämne: [TN] reflow soldering metal backed pcb
Happy New Year and good health for all !!
Is there any who has experience with reflow soldering metal backed pcb's?
The metal is aluminium, the insulation is FR4, the solder is lead free.
I am looking for a process window.
Regards,
Peer Langeveld
Consultant Soft Soldering
5502 VH8
The Netherlands
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|