In a message dated 1/9/2008 12:43:52 AM Pacific Standard Time,
[log in to unmask] writes:
Hi yaself!
Njetskij, sorry, what I aimed at is a very recent invention, Stablcor has
existed for a decade.
If there is a NASA guy among the TNetters, he may find by searching at
'carbon cloth PWB' or 'carbon reinforced boards' or something like.
Inge
Hi Inge
Carbon fiber core PCBs were built for a project at Boeing in the 1980-81
time frame.
Joe
**************Start the year off right. Easy ways to stay in shape.
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------