4% rings a bell. can't remember when and where got the number....jk
On Jan 8, 2008, at 3:13 AM, Hernefjord Ingemar wrote:
> How could you write a warpage spec with all hundreds variants of
> boards,
> from a single layer to twelve, size from an inch to fifty, various
> prepregs, variations of components, weight variations and a lot more
> design matters? Seems a little unrealistic to me. We looked for such a
> spec when we started the production of large brass backed teflon
> boards,
> but we did not find a suitable spec.
> Inge
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
> Sent: den 7 januari 2008 22:10
> To: [log in to unmask]
> Subject: Re: [TN] Warpage of components
>
>
> Most BGAs are built on a FR4-8 circuit board. Like any other FR-4 pwb,
> they can warp for all of the same reasons, copper imbalance, excess
> moisture content, etc. only it is easier for them to do because
> they are
> built on .031 thick material.
> I do find that pre-baking at 105 for 3-5 hours helps quite a bit,
> and a
> longer soak time at reflow also seemed to help. But some BGAs like a
> Universal 366 ball and the infamous Altera 484 I sometimes cannot do a
> darn thing to get them to reflow properly. Likewise, some BGAs do not
> have the potting over the top of the die fully cured, and it tends to
> shrink during reflow. Not much you can do except use shims. But try
> baking first.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
> Sent: Monday, January 07, 2008 2:29 PM
> To: [log in to unmask]
> Subject: Re: [TN] Warpage of components
>
> Thanks, Guy. That's what I told my VP, but he was not inclined to
> believe me.
> Bev
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
> Sent: Monday, January 07, 2008 3:28 PM
> To: [log in to unmask]
> Subject: Re: [TN] Warpage of components
>
> Got a BGA warping on you?
>
> We saw this problem on an Altera Flex484. A contact at Lucent put
> me in
> touch with a package designer at Altera. With his advice we were
> able to
> develop a reflow profile and rework procedure that worked with the !
> @?%%
> thing.
>
> We could not find a JEDEC spec with which to beat the supplier.
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
> Sent: Monday, January 07, 2008 9:30 AM
> To: [log in to unmask]
> Subject: [TN] Warpage of components
>
> Technetters,
>
> Are there any IPC or JEDEC specs that talk about component warpage AT
> REFLOW TEMPERTURES?
>
> Bev
>
> RIM
>
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential
> information, privileged material (including material protected by the
> solicitor-client or other applicable privileges), or constitute
> non-public information. Any use of this information by anyone other
> than
> the intended recipient is prohibited. If you have received this
> transmission in error, please immediately reply to the sender and
> delete
> this information from your system. Use, dissemination,
> distribution, or
> reproduction of this transmission by unintended recipients is not
> authorized and may be unlawful.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily
> halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily
> halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential
> information, privileged material (including material protected by the
> solicitor-client or other applicable privileges), or constitute
> non-public information. Any use of this information by anyone other
> than
> the intended recipient is prohibited. If you have received this
> transmission in error, please immediately reply to the sender and
> delete
> this information from your system. Use, dissemination,
> distribution, or
> reproduction of this transmission by unintended recipients is not
> authorized and may be unlawful.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily
> halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily
> halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|