http://www.smta.org/files/oregon_chapter_presentation0905.pdf
Of course I did nor finish my investigation yet.
But for Richard here is a paper (a little outdated), but with good pictures
for each type of voids.
After all, seeing is believing.
Thank you all again.
Gaby
----- Original Message -----
From: "Stadem, Richard D." <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, January 30, 2008 2:59 PM
Subject: Re: [TN] Microvoids immersion silver
Thank you (once again) Werner, Dave, and Vlad for educating me. Your
information is invaluable.
-----Original Message-----
From: Igoshev, Vladimir [mailto:[log in to unmask]]
Sent: Tuesday, January 29, 2008 3:46 PM
To: TechNet E-Mail Forum; Stadem, Richard D.
Subject: RE: [TN] Microvoids immersion silver
Richard,
Kirkendall effect is not specific to the noble metals and it's has
nothing to do with the "Champaign" voids either :-) Here is a brief
description of the effect:
"The Kirkendall effect is the migration of markers that occurs when
markers are placed at the interface between an alloy and a metal, and
the whole is heated to a temperature where diffusion is possible; the
markers will move towards the alloy region. For example, using
molybdenum as a marker between copper and brass (a copper-zinc alloy),
molybdenum atoms will migrate towards the brass. This is explained by
assuming that the zinc diffuses more rapidly than the copper, and thus
diffuses out of the alloy down its concentration gradient. Such a
process is impossible if the diffusion is by direct exchange of atoms."
Regards,
Vladimir
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, January 29, 2008 2:31 PM
To: [log in to unmask]
Subject: Re: [TN] Microvoids immersion silver
Werner and Don.
I was always under the impression that Kirkendahl voiding was a result
of the noble metal's (in this case, silver) nucleation through the SJ. I
always thought that this was a time-variable migration. I understand how
all of the process variables described in Werner's response will affect
or support the eventual void formation, but I would not expect Gaby to
find anything in microsections taken immediately after soldering. Would
it not make more sense to thermally cycle the SJs in order to facilitate
the nucleation prior to microsectioning?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Tuesday, January 29, 2008 12:35 PM
To: [log in to unmask]
Subject: Re: [TN] Microvoids immersion silver
Hi Gaby,
I take it what you are seeing are 'champagne voids.'
Voids like these are 'encouraged by rough topography copper, excessive
Ag thickness, some solder paste choices and rapid cool-down after
reflow. But as Donald Cullen says in his comprehensive paper, it
"requires the "Perfect Storm"
of a rather contrived combination of parameters" to produce planar
micro-voiding.
Well Gaby, now you know it-you are "Perfect." ;-)
Werner
**************
Start the year off right. Easy ways to stay in shape.
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|