We have approved and used it as a Pb-free solder paste for ~ 3 years
without issue as an EMS provider for medical, automotive and industrial.
I would consider anything <0.05% as halide free. Note that table 1.1 in
J-Std-004 calls out "0.0%" as being in the "0" flux type category. Lots
of astute people in that original document committee. It could have been
written as "0.0X%" but wasn't.
Rich K / GTS
847-621-7310
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Friday, January 18, 2008 1:44 PM
To: [log in to unmask]
Subject: [TN] L0 flux classification
Does anyone have experience with Senju ECO solder paste M705-GRN360-K2-V
I have a data sheet that says the flux has a maximum of 0.02 (mass%)
Chlorine.
Would that translate to Halide free? There is not much on this stuff in
English.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|