TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Eric Castonguay <[log in to unmask]>
Date:
Wed, 16 Jan 2008 14:37:44 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Simonik, Dave R. (David)" <[log in to unmask]>
Subject:
From:
"Simonik, Dave R. (David)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Eric wrote: 

  "We did this, but still have hard time to differentiate the TinLead
from the white ceramic substrate because the contrast is so light. Any
idea how to proceed?" 

  You might be able to employ some filters with your camera. A
polarizing filter will help to remove the reflections from the non
metallic surface of the ceramic, while maintaining the reflections from
the metallic surfaces. I use a radial polarizer when photographing
outdoors. The filter deepens the blue in the sky, and removes
reflections from bodies of water or window panes. Check out 'Using
Filters in Machine Vision', and 'Contrast Enhancement Through Filtering'
in the attached guide.

Dave Simonik
Process Technician
Sanmina SCI Corp.
Owego NY pcb Division

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric Castonguay
Sent: Wednesday, January 16, 2008 2:05 PM
To: [log in to unmask]
Subject: Bent leads on CCGA - Inspect with Panasonic CM602

Dear Technetters,
Is anybody have some experience of placing CCGA with P&P Panasonic
CM602? 
So far, we had placed hundreds of them but we still did not find a way
to inspect them efficiently for bent leads. We do have a side lighting
camera mounted in the machine. Our service engineer told us that the
reference code must be changed to a BGA type of part. By doing this,
each post is recognized to ensure the leads are straight. We did this,
but still have hard time to differentiate the TinLead from the white
ceramic substrate because the contrast is so light. Any idea how to
proceed? 

We have no way right now the prevent bent leads unless inspecting the
raw parts in the tray magazine before running the line. And we don't
like to do this since there is high risk of damaging the leads by
manipulating the CCGA.

Regards,
Eric Castonguay, process eng.


Legal Disclaimer:
The information contained in this message may be privileged and
confidential. It is intended to be read only by the individual or entity
to whom it is addressed or by their designee. If the reader of this
message is not the intended recipient, you are on notice that any
distribution of this message, in any form, is strictly prohibited. If
you have received this message in error, please immediately notify the
sender and delete or destroy any copy of this message

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use by the addressee(s) named herein and may contain legally privileged and/or confidential information. If you are not the intended recipient of this e-mail message, you are hereby notified that any dissemination, distribution or copying of this e-mail message, and any attachments thereto, is strictly prohibited.  If you have received this e-mail message in error, please immediately notify the sender and permanently delete the original and any copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS NOT INTENDED AS A SUBSTITUTE FOR A WRITING.  Notwithstanding the Uniform Electronic Transactions Act or the applicability of any other law of similar substance and effect, absent an express statement to the contrary hereinabove, this e-mail message its contents, and any attachments hereto are not intended to represent an offer or acceptance to enter into a contract and are not otherwise intended to bind the sender, Sanmina-SCI Corporation (or any of its subsidiaries), or any other person or entity.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2