Bill,
You are welcome. But I would like to emphasize the point of how important
the design aspects of the assembly are to the decision of whether to dip
vs. spray. IF, and that is a big IF, your designs and designers can
support moving all of the non-coated components, like connectors to one
end of the board, then Dipping becomes a very attractive option for the
reasons that Graham stated. For many of our assemblies here, which deal
with geometry dependent RF circuitry, or other complex circuitry that has
to be in the middle of the board, we can't effectively dip, at least
without extreme masking measures.
Doug Pauls
Rockwell Collins
Bill Kasprzak <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/03/2008 07:49 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bill Kasprzak <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Looking for Coating Comparison
Graham and Doug ,
Thanks for your help and pointers.
All I'm looking for at the moment was a resource that indicates better
coverage for Dipping vs Spraying.
Intuitively I realize that this is the case, but I need a source that
actually states that this is the case.
If we pursue dipping equipment, I will definitely look for pointers.
Thanks again.
Graham Naisbitt <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/03/2008 06:11 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Graham Naisbitt <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Looking for Coating Comparison
Hi Bill
Thanks for the intro Doug and Happy New Year everyone.
There was indeed a comparison study done by IVF in Sweden led by Dr
Per-Erik Tegehall in the late 80's early 90's. I can pretty much
summarise:
Dip v Spray - If you can locate all components that shouldn't be
coated onto one edge of the assembly (to eliminate masking) then logic
says the best and cheapest way to conformally coat is to dip. Because
you coat both sides at the same time, and the board edges, you can run
anything up to around 40 units per dip. This would yield something
more than 600 assemblies per hour from a basic system.
The tricks - apart from the masking issue are:
Immersion depth must be really accurately controllable.
Speed in should be less than 12 inches (30 cm in new money) per MINUTE
to ensure that the coating penetrates under all of the components.
Withdrawal speed should be slower then the cascade effect of the
coating, generally less than 4 inches (10 cm in new money) per MINUTE
to give you the desired thickness. Material viscosity and solids
content affect this.
Make the dip stroke as smooth as possible to give best coverage
without runs and drips and minimise the "wedge effect" at the bottom
edge.
I can give you a coating film down to 120nm at better than ±5% - you
simply cannot achieve this sort of coverage/accuracy when spraying.
Reason to spray? Masking is easier - it's a shield not a barrier.
Reason to use a robot? Masking is minimised but never eliminated.
Reason to Dip? Better coverage and save money but get your designer to
heed the production process.
Hope this helps - if you need more I do have a Conformal Coating Facts
& Data Book I can send you - ask off-line.
Kindest regards
Graham Naisbitt
[log in to unmask]
www.gen3systems.com
Phone: +44 (0)12 5252 1500
Mobile: +44 (0) 79 6858 2121
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Gen3 Systems Limited
Unit B2, Armstrong Mall
Southwood Business Park
Farnborough Hampshire
GU14 0NR - UK
ENGINEERING RELIABILITY
IN ELECTRONICS
Registered Number: 4639449 (England & Wales). Registered Office as
above.
DISCLAIMER : This message is intended only for the use of the
individual or entity to which it is addressed and may contain
information which is privileged, confidential, proprietary, or exempt
from disclosure under applicable law. If you are not the intended
recipient or the person responsible for delivering the message to the
intended recipient, you are strictly prohibited from disclosing,
distributing, copying, or in any way using this message. If you have
received this communication in error, please notify the sender and
destroy and delete any copies you may have received. Any views or
opinions presented in this email are solely those of the author and
might not represent those of Gen3 Systems Limited. Although Gen3
Systems Limited has taken reasonable precautions to ensure no viruses
present in this email, Gen3 Systems Limited can not accept the
responsibility for any loss or damage arising from the use of this
email or attachments.
On 2 Jan 2008, at 16:06, Bill Kasprzak wrote:
> Happy New Year to one and all.
>
> It sure was difficult this morning to start the old grind again.
> Well, I'm
> thinking just 8 more years and I hope I can retire, so the end is in
> sight.
>
> I'm looking into whether there has ever been a comparison study done
> that
> gives the pros and cons for conformal coating application. I'm sure
> there
> has been because I remember reading about it. Right now I can't seem
> to
> find any information on it.
>
> Specifically, I'm looking for something that states that Dip coating
> provides better coverage than Spray coating.
>
> Any suggestions? Thanks in advance for any responses.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]
> : SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]
> : SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask]
> or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|