Well now Dave, it depends.
What do you mean by medical application? Is this being inserted inside
someone? An electrical device exposed to bodily fluids? High reliability
or life critical function?
I would probably start with Taiyo PSR-4000. Works pretty good on our high
reliability stuff.
Doug Pauls
Dave Seymour <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/02/2008 03:12 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Dave Seymour <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] liquid imageable soldmask
Does anyone have any recommendations for a photo imageable solder
mask that can be used in a medical application?
Thanks
dave
Dave Seymour, CID+
Catapult Communications Inc.
800 Perimeter Park Dr, Suite A
Morrisville, NC 27560
Direct: (919)653-4249
Main: (919)653-4180
Fax: (919)653-4297
[log in to unmask]
*********************************************************************************************************
"This e-mail (and any attachments) is confidential and privileged
information of Catapult Communications"
*********************************************************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|