And what some call a "gold flash" in Europe might be something different
than what someone
calls a "gold flash" in the US. (One could be ImmAu and one could be
Electroplated Gold)
Regardless..as pointed out in the email string there is a few ways to
measure the deposited
Nickel thickness.
Happy Holidays,
Groovy
----- Original Message -----
From: "Hfjord" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Sunday, December 30, 2007 7:26 AM
Subject: [TN] SV: [TN] SV: [TN] Hand Soldering Matte Tin over Nickel Flash
with SnPb Alloy
Correct, flash can't be measured with SEM. My point is a fast and simple
check to see if the layers are thinner than 2-3 micrometers. If you don't
see any tin or nickel with a SEM, then, it is flash, and flash as finish for
a SMT component is foreign for me....and probably most of us. Only flash I'm
used to see is gold flash.
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Yuan-chia Joyce Koo
Skickat: den 30 december 2007 15:03
Till: [log in to unmask]
Ämne: Re: [TN] SV: [TN] Hand Soldering Matte Tin over Nickel Flash with SnPb
Alloy
Can't you use micro-XRF? flash is hard to x-section and detect even
using SEM (unless very good at polishing without smear)... jk
On Dec 29, 2007, at 6:15 PM, Hfjord wrote:
> Nickel flash! You'd better tell us the whole story, e.g. post the
> datasheet
> to Steve or give a link. Agree with George, make Xsection, takes
> half an
> hour with fast acrylic, 600+2500 paper polish, dip a few seconds in
> an acid
> solution, just for making a topographic contrast, put the sample in
> a SEM
> with backscatter detector and see if the layers are thinner than
> let's say
> 2-3 micrometers (you can't do any precision measurements this way).
> If both
> tin and nickel is thinner than that, I'd recommend pulling the
> emergency
> brake and do what George recommended.
>
> So....Christmas is over for many...I'm lucky to have a few days
> more as
> free...ZZZZZZZZZZZZ
>
> Inge
>
> PS. Forgot to tell you, if you are not used to sample preparation:
> use a
> whole bunch of resistors, not just one! There may be variations
> too....
>
> -----Ursprungligt meddelande-----
> Från: TechNet [mailto:[log in to unmask]] För Wenger, George M.
> Skickat: den 28 december 2007 19:05
> Till: [log in to unmask]
> Ämne: Re: [TN] Hand Soldering Matte Tin over Nickel Flash with SnPb
> Alloy
>
> I think the first thing I would do is to determine what p
> Chris,
>
> I think the first thing I would do is to determine what part of the
> component surface I was soldering to by running a trial and by doing
> cross sections. The trial would be to solder side by side a component
> that had formed leads and one that didn't have formed leads. I would
> also cross section two other components (one with formed leads and one
> without)before soldering to see if the soldering problem is due to the
> fact that the forming process exposes nickel in the area that is being
> soldered. I'd also do a third evaluation and us an XRF to measure the
> thickness of the Sn and the Ni on the component leads both before and
> after forming. It might just turn out that you're having
> solderability
> issues because you're soldering to exposed Ni rather than matte Sn.
>
> Regards,
> George
> George M. Wenger
> Andrew Corporation Wireless Network Solutions
> Senior Principal FMA / Reliability Engineer
> 40 Technology Drive, Warren, NJ 07059
> (908) 546-4531 [Office] (732) 309-8964 [Cell]
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Schaefer
> Sent: Friday, December 28, 2007 12:00 PM
> To: [log in to unmask]
> Subject: [TN] Hand Soldering Matte Tin over Nickel Flash with SnPb
> Alloy
>
> Greetings All,
>
> I have a PTH TK type resistor component that is formed to fit an SMT
> geometry land pattern. The component is Pb Free component plated using
> Matte Tin over Nickel Flash. Once the component is soldered it
> exhibits
> non-
> wetting/ poor wetting characteristics thus causing us to rework
> until we
> have
> achieved acceptable results. Of course this is not what I would
> like to
> see
> occur, but unfortunately at this time it is the process. The
> installation process
> is as follows:
>
> - Part is formed using a lead forming tool
> - Is tinned using 25% RMA for 3 seconds and let to dry (somewhat);
> then
> soldered (SnPb tin/ lead alloy) for 3-4 seconds in a 600F bath
> - It is soldered (SnPb tin/ lead alloy) to the cca using a 6ooF solder
> iron tip for
> 2-3 seconds
> - END...
>
> Apparently this has been an issue for years, but just recently was
> brought up
> to our Engineering department. We tin the component to allow for
> improved
> wetting characteristics, but this does not provide much improvement. I
> have
> done some investigation on the internet looking for reports and tests
> performed soldering Matte Tin over Nickel using standard Tin/ Lead
> alloy, but
> have found very little information regarding this. The component
> manufacture
> states our process as described to them 'should work without issue,
> but
> this is
> not the case.
>
> So my questions are what are the issues related to soldering matte tin
> over
> nickel flash with tin/ lead alloy? What hand soldering parameters are
> considered optimal/ ideal with a low-mass matte tin plated component
> considering the information provided? Is it possible to get very
> similar
> results
> using this combination of metallurgies versus using tin/ lead plating
> and solder
> materials?
>
> Any help would be appreciated.
>
> Thank You,
>
> Chris
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ----------------------------------------------------------------------
> ------
> --------------------
> This message is for the designated recipient only and may
> contain privileged, proprietary, or otherwise private information.
> If you have received it in error, please notify the sender
> immediately and delete the original. Any unauthorized use of
> this email is prohibited.
> ----------------------------------------------------------------------
> ------
> --------------------
> [mf2]
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|