Subject: | |
From: | |
Reply To: | |
Date: | Thu, 20 Dec 2007 09:43:47 -0700 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Doug, Sorry, read from the wrong line, it is a polyurethane coating. The propylene is one component of this coating.
Sue
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, December 20, 2007 9:32 AM
To: TechNet E-Mail Forum; Sue Powers-Hartman
Subject: Re: [TN] Parylene Coating Removal
Sue,
What is a propylene coating? Never heard of one of those.
Doug Pauls
Sue Powers-Hartman <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
12/20/2007 10:30 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Sue Powers-Hartman <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Parylene Coating Removal
Bill, we are using a propylene coating for touchup.
From: Bill Kasprzak [mailto:[log in to unmask]]
Sent: Thursday, December 20, 2007 9:23 AM
To: TechNet E-Mail Forum; Sue Powers-Hartman
Subject: Re: [TN] Parylene Coating Removal
Believe it or not, you're not too far off base. We do spot sand blasting with walnut shells.
But whatever the method, it must be abrasive!
Just curious though, how are you touching up the coating on the location being reworked?
We use urethane coating for touch up locations.
[cid:[log in to unmask]]
Sue Powers-Hartman <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
12/20/2007 11:01 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Sue Powers-Hartman <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Parylene Coating Removal
What is the best way to remove parylene coating? Right now the operators
are scraping the coating off the joint enough to allow access with a solder
iron. We would like to find a better way.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|