The amendment page of IPC-6012B 6.2.11.1 can be free download from IPC website. You can see the text and picture description in it. Anyone interested can visit www.ipc.org to search.
Best Regards,
>>> [log in to unmask] 12/18/2007 11:04 AM >>>
IPC-6012B (2007版)3.6.2.11.1 里面有一个"wrap copper "的要求,是2007版的新要求,目前,有中文名。
Best regards with thanks!
CS engineer Eric zhang(俊杰)/QA Dept.
Suntak Multilayer PCB Co.,Ltd
mobile phone:13923405590
Tel:+86-755 26068047ext.803
Fax:+86-755 26068048
e-mail:[log in to unmask]
Addr.:No.1040 Nanshan Rd.,Nanshan Dist.Shenzhen,Guangdong,PRC.
----- Original Message -----
From: [log in to unmask]
To: [log in to unmask] ; [log in to unmask]
Sent: Tuesday, December 18, 2007 10:37 AM
Subject: 回覆: [TGA] (瑞星提示-此邮件可能是垃圾邮件)[TGA] Join TG Asia
铜漆包or漆包管?
Best Regards
Yun, Xunisa ( 黎?yIES030810)
Troubleshooting Room / ICT Team Leader
021-64298888-62340 / Yun.xunisa at inventec.com
英?I?_科技有限公司/?u造二??/生技二部/?a品?S修二?n
------------------------------------------------------------------------------
寄件者: TGAsia [mailto:[log in to unmask]] 代理 俊杰
寄件日期: 2007年12月18日 10:29
收件者: [log in to unmask]
主旨: Re: [TGA] (瑞星提示-此邮件可能是垃圾邮件)[TGA] Join TG Asia
Hi Susan:
do you know what is wrap copper? our company received a complaint form USA just now, we very hope getting some help in the issue.
Best regards with thanks!
CS engineer Eric zhang(俊杰)/QA Dept.
Suntak Multilayer PCB Co.,Ltd
mobile phone:13923405590
Tel:+86-755 26068047ext.803
Fax:+86-755 26068048
e-mail:[log in to unmask]
Addr.:No.1040 Nanshan Rd.,Nanshan Dist.Shenzhen,Guangdong,PRC.
----- Original Message -----
From: Susan Le
To: [log in to unmask]
Sent: Tuesday, December 18, 2007 10:00 AM
Subject: (瑞星提示-此邮件可能是垃圾邮件)[TGA] Join TG Asia
Hello everybody,
I am the laboratories vice director from Microtek (Changzhou) Laboratories. I am very happy to join in the TGAsia.
Best regards,
Susan Le 逸
Microtek (Changzhou) Laboratories
Tel: +86 0519-85487809
Fax: +86 0519-85487810
Email:[log in to unmask]
www.china.thetestlab.com
|
|
|