I haven't heard of anyone measuring flux volume. Don't know what that
would tell you- probably what is more important is areas that are fluxed
but not exposed to the wave solder temperatures. Might ask the flux
vendor about the effects of these residues . The non thermally activated
flux residues on the board might be hygroscopic and cause current
leakage and worse case lead dendrites and/or corrosion.
Tom
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joel Alexander
Sent: Friday, November 30, 2007 4:25 PM
To: [log in to unmask]
Subject: [TN] Wave solder flux volume measurements
Hi guys its me again,
We have a customer that builds power systems for the Telcom companies.
They recently had a field failure on a backplane. It had sever
corrosion.
We process the assembly with a VOC no-clean solder and have never had
issues in the past. The customer indicated that the backplane was in a
damp/moist environment. That is not a good combination for no clean
flux.
I suggested cleaning but they insisted that we monitor our flux volume
to ensure it is at the recommended application volume. I did not really
agree from a reliability standard.
Does anyone out there measure their no clean flux volume on a regular
basis?
Joel Alexander
Quality Assurance Manager
TT APSCO, INC.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|