I'll agree with Miguel. Testing I performed using SN100C alloy and a
test assembly designed to induce solder skips and solder bridges showed
the Soltec machine with the selective debridger was considerably
superior to my present Sn/Pb process.
Gary
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Miguel Vallejo
Sent: Thursday, December 06, 2007 10:22 AM
To: [log in to unmask]
Subject: Re: [TN] Wave solder machine recommendations?
I've had experience with Technical Devices' NuEra, Vitronics Soltec, and
a Chinese made machine for lead-free.
The Vitronics Soltec is by far my first choice.
The TD required too much maintenance and tweaking to maintain acceptable
quality levels.
The Chinese machine gave me problems right out of the box, and proved to
be high-cost of ownership.
I've heard some mfr's are just buying these machines, and selling them
with their name on it. Not the same as building in China and following
the OEM's quality standards.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, December 06, 2007 5:26 AM
To: [log in to unmask]
Subject: [TN] Wave solder machine recommendations?
Morning all!
Just taking a quick poll, who would you recommend as far as wave solder
machine manufacturers taking into account machine performance, machine
quality, and customer support (not necessarily in that order).
We're thinking about a new machine...
Steve Gregory
Production Engineer
OAI Electronics
6960 East 12th Street
Tulsa, Oklahoma 74112
(918) 836-9077 Ext 507
(918) 836-0184 FAX
(918) 706-2779 Cell
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|