Sure it will. Compare with conformal coating on PWBs. Correctly applied the
coating minimizes the migration risk, even if it's not 100% eliminated.
/Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Anat Douek
Skickat: den 4 december 2007 08:11
Till: [log in to unmask]
Ämne: Re: [TN] SV: [TN] FW: shorted feedthus due to silver migration
Thank you for the answer. I know that migration caused by the silver plated
feedthru. The question is if non conductive epoxy which will cover
feedthru body can prevent the short.
Anat
-----Original Message-----
From: Hfjord [mailto:[log in to unmask]]
Sent: Monday, December 03, 2007 11:27 PM
To: [log in to unmask]
Subject: [TN] SV: [TN] FW: shorted feedthus due to silver migration
Silver epoxy does not start migration. Your silver migration is probably
caused by the silver plated feedthroughs. We NEVER us Silver. Our glass
beads have gold flash over nickel over the base metal.
/Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Anat Douek
Skickat: den 3 december 2007 15:09
Till: [log in to unmask]
Ämne: [TN] FW: shorted feedthus due to silver migration
Hi,
I am facing a problem of silver migration with soldered feedthru. The silver
plated feedthrus are soldered to an aluminum housing and +60V is applied to
the feedthru's pin. After period the voltage fall down and silver residues
observed on the glass insulator . These residues caused the pin to short to
the body.
Is epoxy adhesive which will cover the feedthru body , after the soldering,
can be a solution ?
Please advise,
Thanks,
Anat Douek
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|