TECHNET Archives

December 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David Suraski <[log in to unmask]>
Date:
Wed, 19 Dec 2007 08:46:13 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
From:
Phil Nutting <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (107 lines)
David,

Sadly, yes.

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Suraski
Sent: Wednesday, December 19, 2007 8:43 AM
To: [log in to unmask]
Subject: Re: [TN] open letter to solder manufacturers

Do some companies actually print information on the part of the label
that is punched out? That's just completely lacking in common sense. Our
labels don't even cover the spool hole.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Wednesday, December 19, 2007 9:16 PM
To: [log in to unmask]
Subject: [TN] open letter to solder manufacturers

To all the solder wire manufacturers frequenting Technet I'd like to
discuss the following problems and offer some suggested solutions.

The most common form of wire solder is on a roll.  And the most common
form of labeling covers the full end of the roll.  Unfortunately the
part of the label that covers the hole is destroyed and product
information is lost when this label is "punched out" when the roll is
placed on a rack or other holding device the goes through the center
hole of the spool.

With the many alloys and flux chemistries it can get difficult to
differentiate one spool from another when they all have the same color
spool.

My recommendations;

Make a label for the spool that already has the hole punched out and all
the pertinent product information is printed on this "donut" shaped
label, then even at some point in the future we could tell just what is
on the spool.

Standardized on a spool color scheme as simple as green for any
lead-free alloy and white for any tin-lead alloy.  I realize the
complexity of trying to color code every possible alloy and flux
combination so that is why I offer such a simple color scheme.

Lets agree on some simple standards, embrace them and make everybody's
day a little simpler... at least in identifying just what that
mysterious roll of solder is.

Thanks for taking the time to read this.

Best regards,

Phil Nutting
Design for Manufacturing Engineer
Kaiser Systems, Inc.
126 Sohier Road
Beverly, MA 01915
voice: 978-922-9300 x1310
fax: 978-922-8374
e-mail: [log in to unmask]
www.kaisersystems.com

Note: All the information contained in this e-mail and its attachments
is proprietary to Kaiser Systems, Inc. and it may not be reproduced
without the prior written permission of sender.  If you have received
this email in error, please immediately return it to sender and delete
the copy you received.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender.  If you have received this email in error, please immediately return it to sender and delete the copy you received.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2