Yup, that means the housing is inadequate to keep humidity and/or
condensation from the assembly surface. Time for coating.
Doug Pauls
Joel Alexander <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
12/03/2007 09:01 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
Re: [TN] Wave solder flux volume measurements
I do not know the humidity level but from what I can tell from the return
water is condensing to the extent that drops are rolling off the backplane
in some locations
Joel Alexander
Quality Assurance Manager
TT APSCO, INC.
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
12/03/2007 09:46 AM
To
"TechNet E-Mail Forum" <[log in to unmask]>, <[log in to unmask]>
cc
Subject
RE: [TN] Wave solder flux volume measurements
Your Environmental condition was damp/moist. Is that opposed to damp/dry
or dry/moist? It would more helpful to relate it to temperature and
relative humidity with the additional qualifier of standing water or
not.
A general rule of thumb (besides move it before striking with heavy
objects) is that no-cleans should not be used in that application. A
cleanable no-clean or better yet a water soluble flux should be used.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joel Alexander
Sent: Friday, November 30, 2007 2:25 PM
To: [log in to unmask]
Subject: [TN] Wave solder flux volume measurements
Hi guys its me again,
We have a customer that builds power systems for the Telcom companies.
They recently had a field failure on a backplane. It had sever
corrosion.
We process the assembly with a VOC no-clean solder and have never had
issues in the past. The customer indicated that the backplane was in a
damp/moist environment. That is not a good combination for no clean
flux.
I suggested cleaning but they insisted that we monitor our flux volume
to
ensure it is at the recommended application volume. I did not really
agree
from a reliability standard.
Does anyone out there measure their no clean flux volume on a regular
basis?
Joel Alexander
Quality Assurance Manager
TT APSCO, INC.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
ForwardSourceID:NT000C88BE
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|