Loctite 3621 requires a "substantial heat bump" of 150 seconds at 150
deg. C to fully cure. It is designed to adhere to almost any component.
It can be applied with a manual syringe or automated dispenser, does not
seep away but stays in place until cured. It can be cured as part of a
wave solder or reflow process. It has super strong peel strength, is
impervious to most chemicals, and is a very low outgassing single part
epoxy.
Good stuff.
And it does not stink.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Swanson
Sent: Wednesday, November 21, 2007 9:59 AM
To: [log in to unmask]
Subject: Re: [TN] Epoxy application
Peter,
You don't say how many of these you are making, but with that proviso:
1) A single part "chipbonder" or surface mount adhesive like the one
mentioned will require a substantial heat bump to cure.
2) Rather than an epoxy, maybe a methacrylate adhesive would be better -
often less brittle, but good all round adhesion. Something like Araldite
2022 is a two part product, but in a cartridge, so easy to apply. Might
still me a bit smelly through....
3) If you have, or can justify the purchase of the equipment, then a UV
acrylic adhesive does this job well. No mix, fast cure, good adhesion,
choose your viscosity and the right resiliency to give the stress
relief.
Regards,
Peter
--------------------------------------------------------
Peter Swanson [log in to unmask]
INTERTRONICS http://www.intertronics.co.uk
Tel: +44 1865 842842 Oxfordshire, England
INTERTRONICS is dedicated to providing quality material, consumable and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.
Read our news! http://www.intertronics.co.uk/blog/blog.htm
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: 21 November 2007 13:28
To: [log in to unmask]
Subject: Re: [TN] Epoxy application
Hello, Peter
I have a client using Loctite 3621 epoxy in a very similar application.
It bonds to the mylar sleeving very well. Try it.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter L
Sent: Tuesday, November 20, 2007 6:00 PM
To: [log in to unmask]
Subject: [TN] Epoxy application
Hello,
I would like to ask for opinion on an epoxy application. We apply RTV to
bond and secure 2 electronic devices on a PCB.
But after noticing the RTV bond breaking off during vibration test, our
customer has specs in a 5min 2-part epoxy (made by
http://www.devcon.com/techinfo/5_MINUTE_FR.pdf) to replace the RTV. The
problem is that the Devcon epoxy is fast cure, requries 2 part mixing,
and carries a strong, irritating odor. I would like to move away from
using Devcon and expect that there must be more process friendly epoxy
for such application.
The 2 materials to be joined were a flat ferrite inductor and round
capacitor having a PVC sleeve. Due to positioning of the 2 devices there
is generally a ~0.25" gap between them for the epoxy to fill. The epoxy
bead deposit is about .75" long x 0.5" wide. (see following link to the
assembly
http://members.shaw.ca/ppwlee4/Epoxy_appl.JPG)
I am looking for recommendation of a suitable epoxy to allow:
- 5-10 min working life before it starts curing
- process friendly (smell, preferrable no pre-mix)
- good adhesion to the component/PCB surfaces.
Any suggestion is appreciated. Thanks.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|