Hi Graham
No.
Kindest regards
Graham Naisbitt
[log in to unmask]
www.gen3systems.com
Phone: +44 (0)12 5252 1500
Mobile: +44 (0) 79 6858 2121
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Gen3 Systems Limited
Unit B2, Armstrong Mall
Southwood Business Park
Farnborough Hampshire
GU14 0NR - UK
ENGINEERING RELIABILITY
IN ELECTRONICS
Registered Number: 4639449 (England & Wales). Registered Office as
above.
DISCLAIMER : This message is intended only for the use of the
individual or entity to which it is addressed and may contain
information which is privileged, confidential, proprietary, or exempt
from disclosure under applicable law. If you are not the intended
recipient or the person responsible for delivering the message to the
intended recipient, you are strictly prohibited from disclosing,
distributing, copying, or in any way using this message. If you have
received this communication in error, please notify the sender and
destroy and delete any copies you may have received. Any views or
opinions presented in this email are solely those of the author and
might not represent those of Gen3 Systems Limited. Although Gen3
Systems Limited has taken reasonable precautions to ensure no viruses
present in this email, Gen3 Systems Limited can not accept the
responsibility for any loss or damage arising from the use of this
email or attachments.
On 1 Nov 2007, at 17:00, Graham Collins wrote:
> Hi TechNet
> Having a production time crunch, the usual question is being asked
> of me
> - "Do we have to cure the coating for THAT long????"
>
> So - any coating gurus out there (Graham N, are you there?):
> - Humiseal 1A33, per the spec sheet, minimum cure is 20 hours at 190F
> (87.8C).
> Is it possible to cure at a higher temperature for less time, without
> compromising the performance of the material?
>
> Thanks!
> - Graham Collins
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|