TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 21 Nov 2007 13:55:44 EST
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Werner Engelmaier /* <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
Hi Jack,
Even so they do not show directly, you have 8 internal layers plus 2 outer 
layers.
The most striking thing about this PCB is the thickness imbalance between the 
core layers [much thinner] and the prepreg layers [more than double the 
thickness of the core dielectric]. A good design should have these thicknesses 
balanced.
Also, having the prepreg layers so disproportionally thick can impact 
survivability of leadless soldering rocesses and long-term reliability [in severe 
operating environments], because the CTE(z) of the prepreg layers is quite a bit 
larger than the CTE(z) of the core layers, particularly above Tg.



Werner



**************************************
Check out AOL's list of 2007's hottest 
products.

(http://money.aol.com/special/hot-products-2007?NCID=aoltop00030000000001)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2