My experience is that there is a slight cost reduction for ImAg. More
important is the 2-3 day reduction on lead times. YMMV
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Thursday, November 01, 2007 1:58 PM
Subject: ENIG vs. Immersion Silver
Hi All,
What is the general consensus regarding the cost of ENIG versus
Immersion Silver. Can I expect to save any money by switching to
Immersion Silver or, for all practical purposes, is it even?
Thanks in advance,
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
NOTICE: This e-mail transmission (and/or the attachments accompanying it) may contain confidential or proprietary information belonging to DRS Technologies or the sender. The information is only for the use of the intended recipient. If you are not the intended recipient you are hereby notified that any disclosure, copying, distribution or the taking of any action in reliance on the contents of this information is strictly prohibited. Any unauthorized interception of this transmission is illegal under the law. If you have received this transmission in error, please promptly notify the sender by reply e-mail, and then destroy all copies of the transmission.
"This (document/presentation) may contain technical data as defined in the International Traffic In Arms Regulations (ITAR) 22 CFR 120.10. Export of this material is restricted by the Arms Export Control Act (22 U.S.C. 2751 et seq.) and may not be exported to foreign persons without prior written approval from the U.S. Department of State."
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|