Good Morning Sylvain and everyone eles!
I have a few more pictures that were sent to me to post. They are here:
http://stevezeva.homestead.com/files/G_n__fonct_pignard_02_crop.JPG
http://stevezeva.homestead.com/files/G_n__fonct_pignard_closeup_21.jpg
http://stevezeva.homestead.com/files/G_n__fonct_pignard_closeup_35.jpg
WOW, that's a lotsa flux around that QFP! I wonder why the component had the rework done in the first place?
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Sylvain Kaufmann
Sent: Friday, November 09, 2007 2:12 AM
To: [log in to unmask]
Subject: [TN] Flux residues - great balls of fire
Hello technetters,
Sorry for the subject but that's what came to my mind when I faced this case :) I never saw this previously, even when I burnt 2kW/chan amps in rock shows the result was not so catastrophic!
I would be very glad to have your thoughts about some pictures I sent to Steve.
http://stevezeva.homestead.com/files/G_n__fonct_pignard_03_crop.JPG
http://stevezeva.homestead.com/files/G_n__fonct_pignard_closeup_16.jpg
Additional pictures has been sent to Steve this morning (relatively to my location).
Here is the case:
One customer from us came up with one function generator with its case open; he opened it because it stopped working and had a bursty odor (smell?) and he wanted to see what was this odor and if he could change a fuse and let it work again. When he saw what was on the board, he came up to me to take pictures and have little explaination of what went wrong on this board. The customer bought this generator one year and a half ago, so it's still under guarantee, but he wanted to protect himself against a manufacturer's complain that could have said: "you did a short on the output, this repair doesn't fall into guarantee scope, so you pay for it" (now that he opened the case, maybe the guarantee is allready gone, but whatever). This generator has not been used a lot, understand it's not a generator that is installed in an automatic test setup that runs 24h a day.
The facts:
- Presence of flux residues on both sides
- Presence of several different copper oxydes (I don't know their english correct names, but the green ones, the green gelatin like ones, the red ones)
- PCB's temperature increased up to at least 300°C or so
- Generator was not working in a harsh environment; it was lying on a table in engineer lab, so, except if there was some fog from the open window near to the table, this generator never saw external humidity :)
My guess:
- The manufacturer/assembler did a rework/touchup on a QFP on the top side of the PCBA; to perform it, the operator used a very active flux that he spread around the component he wanted to rework; some of flux went on the other side through the PCB vias.
- Then the generator worked properly for about one year and a half, but during this time, some aggressive compound eat gently the copper barrel in several vias, leading to a increase of the barrel electric resistance, up to the time the resistance was so high that the dissipated power elevated the temperature to about 300°C.
- Or this could be the result of electromigration and a hard short-circuit that happened on the board.
- This part of the design has a control loop and power was first provided by control electronics up to the time this power could not be dissipated anymore and the PCB broke and so the generator stopped working
My concern:
- As I see this happening without other factors than ones related to assembly (no humidity, no high voltage, no thermal shocks, no vibrations), I wonder what are the circumstances that lead to such destruction; is it only the flux chemistry? If I see some green gelatine like copper oxydes in some vias on one of our board, should I consider that this extreme end could happen to my product? Is it one isolated case (PCB destruction with risk of fire) or is it how it will allways end? Etc etc
Thank you for your inputs and have a nice Friday sly
S. Kaufmann
************************************************************
Sylvain Kaufmann
CERN / European organisation for nuclear research Site de Meyrin
1211 Geneva 23
Switzerland
Dpt: TS-DEM-WS (int mail J06600)
Phone: +41 22 767 37 02
Fax: +41 22 766 87 77
E-mail: [log in to unmask]
Web: www.cern.ch
http://cern.ch/dem
************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|