Dear Badri,
If you specified 70/70/70/70 microns of copper and referred to IPC-A-600G
for acceptability, then you return the boards to the manufacturer. He should
replace them with what you ordered.
As you are at it, you should check the copper thickness within the holes
that are connecting to the inner layers to make sure there is enough Copper
plating to enable electrical conduction of high power as well. Typically 30
microns plating as 20 won't usually do.
As for the assembled parts, see how to negotiate with your supplier if he is
faulty.
For this type of PCBs, there more to check as well
But IMO, your RFQ and the order itself should have the details of the
specific spelled out for your supplier.
Meilleures Salutations
Very Best Regards
Roland
www.PCBspecialist.com
Roland Jaquet
14 Champ Budin
1258 Perly, GENEVA
SWTZERLAND
GSM+41-79-203-3723
"Quality is best measured not by the return of the products but by the
return of the customers"
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de badri
Envoyé : mercredi, 7. novembre 2007 08:36
À : [log in to unmask]
Objet : Re: [TN] Delamination of lead free PCBs
Dear Technetters,
During production of the XXXX boards, we found that that the inner tracks
were getting opened(discontinuity) and nearly 50% of the boards were failing
during the testing.
On further analysis we found that the copper thickness of the inner layers
were less when compared to the outer layers. On confirmation with PCB
supplier we found that the Finish Cu thickness was maintained at 70/35/35/70
micron whereas our gerbers sent to supplier calls for 70/70/70/70 micron.
The issue was discussed with our customer and they informed that they cannot
accept the boards since they are using the boards for a high power
applications(2.5KVA) and the tracks cannot withstand this kind of voltage
which will cause field failures.
Please find the below information of the PCBs and the PCBAs which has to be
scrapped because of this.
Assembled 50nos
Assembled 110nos
We and our customer are now in a very desparate situation and we need to
turn up ASAP. Now the details are as follows:
Process: ROHS
Usage: UPS
No. of layers: 4
How do I salvage the assembled boards?
Thanx
Badri
Thanks&Regards,
Dinesh
Disclaimer:
===========
This E-mail may contain privileged information and is intended solely for
the addressee. Any unauthorized use or dissemination of this message in
whole or in part is strictly prohibited. If you have received this mail by
mistake, please inform us immediately and delete this mail. Any information
expressed in this mail does not necessarily reflect the views of Avalon
Technologies (P) Ltd .
Avalon Technologies(P) Ltd shall not be responsible nor liable for the
proper and complete transmission of the information contained in this
communication nor for any delay in its receipt or damage to your system.
Avalon Technologies(P) Ltd does not guarantee that the integrity of this
communication has been maintained nor that this communication is free of
interceptions or interference.We have taken precautions to minimize the risk
of transmitting software viruses, but we advise you to carry out your own
virus checks on any attachment to this message. We cannot accept liability
for any loss or damage caused by software viruses.
Thank you for your cooperation
AVALON TECHNOLOGIES MAY MONITOR ALL INCOMING AND OUTGOING MAILS.
****************************************************************************
****************************************************************************
****************************************************************************
****************************************************************************
****************************************************************************
****************************************************************************
****************************************************************************
****************************************************************************
****************************************************************************
****************************************************************************
*********************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|