TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0 (Apple Message framework v752.3)
Sender:
X-To:
Date:
Tue, 6 Nov 2007 18:31:48 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Subject:
From:
Graham Naisbitt <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
<000001c82095$474be030$6601a8c0@smw626e71658ad>
Content-Type:
multipart/mixed; boundary=Apple-Mail-54--829139876
Parts/Attachments:
text/plain (1617 bytes) , text/plain (5 kB)
Hi Inge

I shall try to remember to ask about the components in Vegas, but  
don't bet on it.

As regards the coating, we had a similar question posed many years  
ago by an avionics manufacturer. As we considered the Tg might be too  
low with HumiSeal 1B31, they tried and switched to HumiSeal 1B73.  
Still an acrylic with the benefits thereof, but a slightly higher Tg.

However, IT DEPENDS™ (Cha Ching!) on the amount of particulate matter  
that you are trying to resist - can the enclosure be improved? Most  
coatings have, by the nature of their task, to be soft and pliable.  
However, 1A20 might just do what you are looking for, but its a  
******* to work with.

As for Dewey - he's by far the PUNNIEST man I know.

Kindest regards
Graham Naisbitt

[log in to unmask]

www.gen3systems.com

Phone: +44 (0)12 5252 1500
Mobile: +44 (0) 79 6858 2121


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



Gen3 Systems Limited Unit B2, Armstrong Mall Southwood Business Park Farnborough Hampshire GU14 0NR - UK ENGINEERING RELIABILITY IN ELECTRONICS Registered Number: 4639449 (England & Wales). Registered Office as above. DISCLAIMER : This message is intended only for the use of the individual or entity to which it is addressed and may contain information which is privileged, confidential, proprietary, or exempt from disclosure under applicable law. If you are not the intended recipient or the person responsible for delivering the message to the intended recipient, you are strictly prohibited from disclosing, distributing, copying, or in any way using this message. If you have received this communication in error, please notify the sender and destroy and delete any copies you may have received. Any views or opinions presented in this email are solely those of the author and might not represent those of Gen3 Systems Limited. Although Gen3 Systems Limited has taken reasonable precautions to ensure no viruses present in this email, Gen3 Systems Limited can not accept the responsibility for any loss or damage arising from the use of this email or attachments. On 6 Nov 2007, at 16:51, Hfjord wrote: > I think D is a Deceptive rogue. Are you sure it was his credit > card? May > been his library id or a plastic card for an automatic car washing. > I vote > on D, he will play a trick on you. Have a look on your hotel bill > before > checking out or something like..looking forward to hear about D's > practical > joke. > > When you guys visit APEX, would you ask something for me, or maybe > you have > an answer already. About SMT ceramic capacitors, tantalum chip > capacitors > and ceramic potentiometers: what is the maximum-number-of-temp-cycles > specification that exists for -40/+125 Centigrades? We need test > much, much > more than 500 cycles. > > That was one question, the other one is this: what is the 'best' > conformal > coating to avoid dust and particles to stick in the coating's > surface after > long periods in +50 Centigrades ambient? We use an acrylic coating at > present, good in most aspects, but after long exposure to dusty and > hot > environment, the coating surface can be used as a scotchbrite, to > use an > exaggeration. Especially sand particles are hard to remove. > > /Inge > > -----Ursprungligt meddelande----- > Från: TechNet [mailto:[log in to unmask]] För Graham Naisbitt > Skickat: den 6 november 2007 12:51 > Till: [log in to unmask] > Ämne: Re: [TN] [NTC] Dewey and Graham > > It's my dry sense of humour! > > Anyone care to guess the odds on my meeting Dewey at APEX in Las > Vegas and being able to sign the bar bill using his credit card? > > It's happened before.... > > Graham N > > > > On 5 Nov 2007, at 14:02, Whittaker, Dewey (EHCOE) wrote: > >> Admit it; I'm finally getting to you. From the superfluous >> soliloquy on >> the solderability question to the succinct and monosyllabic answer on >> cure. >> Dewey >> >> -----Original Message----- >> From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt >> Sent: Thursday, November 01, 2007 10:45 AM >> To: [log in to unmask] >> Subject: Re: [TN] curing my conformal coating >> >> Hi Graham >> >> No. >> >> Kindest regards >> Graham Naisbitt >> >> [log in to unmask] >> >> www.gen3systems.com >> >> Phone: +44 (0)12 5252 1500 >> Mobile: +44 (0) 79 6858 2121 >> >> >> --------------------------------------------------- >> Technet Mail List provided as a service by IPC using LISTSERV 15.0 >> To unsubscribe, send a message to [log in to unmask] with following >> text >> in >> the BODY (NOT the subject field): SIGNOFF Technet >> To temporarily halt or (re-start) delivery of Technet send e-mail to >> [log in to unmask]: SET Technet NOMAIL or (MAIL) >> To receive ONE mailing per day of all the posts: send e-mail to >> [log in to unmask]: SET Technet Digest >> Search the archives of previous posts at: >> http://listserv.ipc.org/archives >> Please visit IPC web site >> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional >> information, or contact Keach Sasamori at [log in to unmask] or >> 847-615-7100 >> ext.2815 >> ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following > text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/ > archives > Please visit IPC web site http://www.ipc.org/contentpage.asp? > Pageid=4.3.16 > for additional information, or contact Keach Sasamori at > [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------

ATOM RSS1 RSS2