Then I would be curious to know if your friend includes total defects
found at all those stations when compiling the DPMO:
1-Visual Inspection
2-X-Ray inspection
3-ICT/ Flying Probe
The frequency or time period to which they measure themselves is also
key (weekly DPMO, bi-weekly or one month period).
A DPMO of 10-15 is achievable at only ICT/FP (taking into account enough
test coverage) but including all stations listed above, this is amazing.
They certainly have a well trained and experienced workforce to achieve
this. This corresponds to 4.3 Sigma or 8.5 ppm (defective part per
million)!!! We're at 3.9 Sigma and I consider it very good. Our
corporation wants 4.5 though.
Regards,
Eric
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: 30 octobre 2007 14:47
To: [log in to unmask]
Subject: Re: [TN] World class DPMO
In a message dated 10/30/2007 11:45:38 AM Eastern Daylight Time,
[log in to unmask] writes:
I don't think they are counting everything.
I can assure that they are and they are quite thorough about it. I
have been hired in the past as an auditor of their process and quality
documentation, as well as a trainer for certain functions in their
organization. The numbers are quite real, not padded, nothing omitted,
possibly even conservative in certain areas.
Jon Moore
************************************** See what's new at
http://www.aol.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Legal Disclaimer:
The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|