Hello,
I would like to ask for opinion on an epoxy application. We apply RTV to bond
and secure 2 electronic devices on a PCB.
But after noticing the RTV bond breaking off during vibration test, our
customer has specs in a 5min 2-part epoxy (made by
http://www.devcon.com/techinfo/5_MINUTE_FR.pdf) to replace the RTV. The
problem is that the Devcon epoxy is fast cure, requries 2 part mixing, and
carries a strong, irritating odor. I would like to move away from using Devcon
and expect that there must be more process friendly epoxy for such
application.
The 2 materials to be joined were a flat ferrite inductor and round capacitor
having a PVC sleeve. Due to positioning of the 2 devices there is generally a
~0.25" gap between them for the epoxy to fill. The epoxy bead deposit is
about .75" long x 0.5" wide. (see following link to the assembly
http://members.shaw.ca/ppwlee4/Epoxy_appl.JPG)
I am looking for recommendation of a suitable epoxy to allow:
- 5-10 min working life before it starts curing
- process friendly (smell, preferrable no pre-mix)
- good adhesion to the component/PCB surfaces.
Any suggestion is appreciated. Thanks.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|