Hi Tom,
We have been using a couple of wire solders that have worked well. They are Kester 275 and Aim Glowire. Both are SAC305 no-cleans.
Thank you,
Paul Black
Manufacturing Engineer
Kronos Incorporated
p: 978.947.1520
f: 978.244.0568
www.kronos.com
Experts at Improving the Performance of People and Business(tm)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Tom P. Hummel
Sent: Monday, October 08, 2007 3:39 PM
To: [log in to unmask]
Subject: [TN] RoHS wire solder
I have been assigned the task of getting samples of RoHS compliant wire
solder to evaluate. I was wondering what brands and types of solder are
being used in the market. Does anyone have a preference /
recommendation for RoHS wire solder?
Thomas P. Hummel
Carlton Industries Corp
[log in to unmask]
Phone 203-288-5605
Fax 203-288-9202
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|