This one should be easy enough for Friday.
I've got a drawing calling out the following material:
GE062 C2/C2 1A per MIL-P-13949
I've worked it out so far to be Type GE 0.0620 thick (they left out a 0),
with 2 oz copper on each side.
I can't figure out the 1A. I think it should be A1 for pits/dents class A,
and class 1 for thickness tolerance.
Does this sound right? Also, has anything replaced Mil-P-13949? Is type GE
material commonly available?
Thanks!
Eric Kalgren
Electrical Engineer
Cobham Defense Electronic Systems
Continental Microwave Division
11 Continental Drive
Exeter, NH 03833 USA
Tel: 603-775-5200
Fax: 603-775-5201
E-mail:[log in to unmask]
Website: <http://www.cobhamdes.com/> http://www.cobhamdes.com
<mailto:[log in to unmask]>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------