We clean most of our boards that have no clean flux residues prior to
coating. Concurrently we implemented a Asymtek coating machine.
Fields complaints have reduced significantly.
You aren't just cleaning flux residues - unless your operators are
wearing gloves or finger cots, you've got skin oils on your boards, and
maybe other stuff that you don't know about.
Blair
---------------------------------------------------