Assuming the design has a sufficient 'anti-pad' clearance on the plane
layers spacing to adjacent conductors should not be an issue. Class III
allows .003" maximum. Unusual though that the glass is sheared so far
back. There is some indication of drill tear-out though. I wonder if
the mystery material between layers 4 and 5 has anything to do with
this? Ian
---------------------------------------------------