Hi Inge
Badly drilled holes
- To fast feeding during drilling
- Old drills
No a priori a bad thing.
Possible effects:
- Defects in the Cu- plating leading to sponge solder
- Microcracks along glass fibres promoting Cu- filament growth.
Have a great day
Guenter
_____________________________________________________
EMPA
Swiss Federal Laboratories for Materials Testing and Research
Centre for Reliability
Guenter Grossmann, Senior Engineer
8600 Duebendorf
Switzerland
Phone: xx41 44 823 4279
Fax : xx41 1 823 4054
mail: [log in to unmask]
_____________________________________________________
>>> Hfjord <[log in to unmask]> 10/01/07 7:11 pm >>>
Broken glass fibers caused by poor tooling parameters is my first thought.
The loss of fibers leaves a small cavity that will be filled by Copper,
sometimes even by solder. I assume, that the preparation is correctly done,
so we can exclude smear.
I think you can sleep tonight, this failure can be easily fixed with a fresh
diamond tool in your Excellon.
If you use laser drilling, the above is not valid.
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Jack Olson
Skickat: den 1 oktober 2007 18:56
Till: [log in to unmask]
Ämne: [TN] Is This a BAD Thing?
I'm not accustomed to looking at reliability issues,
(my designs are usually so perfect... (grin))
so every time I see an X-Ray or a cross-section
I get nervous wondering what I'm actually seeing.
Can anyone explain what the following picture means?
http://www.frontdoor.biz/PCBportal/208what.jpg
onward thru the fog,
Jack
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|