TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 23 Oct 2007 15:22:32 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (48 lines)
Hi Linda,

this kind of information is written in the TDS of most pastes, 3 days is pretty common. If you cannot find it, I would call the manufacturer.

Regards,

Ioan

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Linda Langley
Sent: Tuesday, October 23, 2007 2:40 PM
To: [log in to unmask]
Subject: [TN] cleaning concerns


 
Can anyone tell me or direct me to documentation that specify how long flux residue from WS609 63/37 can be left on a board before washing?
 
I was informed that it could be left on for 7 days . 
 
Linda Langley 
Jabil Circuit 
Training Specialist 
(248) 292-6176 
 
CONFIDENTIALITY NOTICE: The information contained in this electronic communication, including any attachments, is confidential information, is intended only for the use of the recipients named above, and may be legally privileged. If the reader of this message is not an intended recipient, you are hereby notified that any review, use, dissemination, distribution or copying of this communication, or any of its contents, is strictly prohibited. If you have received this communication in error, please notify us immediately of the error by return e-mail and please permanently remove the original message and any copy of it from your system. Nothing herein is intended to constitute an electronic signature or consent. Thank you
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2