We tried many no-clean rosin-free core and lead-free alloy (SAC305 or 387)
wires, no serious preference for any among the operators in terms of
performance (but unanimous that they were harder to use than leaded wires),
but they liked the Alpha product best because it was on a green plastic reel
and thus easily distinguished from any Sn63Pb37 wire reels still in use for
repairs of older product. This was as good a reason as any so we went with
Alpha FT2002 SAC305. Whatever you choose, make sure your supplier provides
a licence paid version if you use a patented alloy though
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------