TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Wed, 10 Oct 2007 06:33:23 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, N Burtt <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="windows-1252"
From:
Parts/Attachments:
text/plain (19 lines)
We tried many no-clean rosin-free core and lead-free alloy (SAC305 or 387) 
wires, no serious preference for any among the operators in terms of 
performance (but unanimous that they were harder to use than leaded wires), 
but they liked the Alpha product best because it was on a green plastic reel 
and thus easily distinguished from any Sn63Pb37 wire reels still in use for 
repairs of older product. This was as good a reason as any so we went with 
Alpha FT2002 SAC305. Whatever you choose, make sure your supplier provides 
a licence paid version if you use a patented alloy though

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2