TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 9 Oct 2007 15:10:02 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
Phil Nutting <[log in to unmask]>
Parts/Attachments:
text/plain (38 lines)
Hello Technetters,

Let me see if I can explain the problem.  We build some PTH boards with
4 oz. copper and connect some high power IGBT devices with thermal
reliefs on the pads.  In the past with tin/lead everything worked well.
More of our designs are being converted over to RoHS (SAC 305).  It
appears we are not getting as much flow through or wetting on these
devices.  So there is a two fold concern.  During a specific failure
mode the thermal reliefs act like a fuse causing arcing until enough
copper vaporizes to make a large enough gap that the voltage can no
longer jump. One solution is remove the thermal reliefs.  Part two is
the amount of current passing through the PTH.  We can't rely on the
barrel for full current carrying capacity so 100% barrel fill is desired
with a good fillet top and bottom.  Here is where we are having issues
with RoHS solder not fully wetting or filling the PTH.

I'm concerned that removing the thermal reliefs will generate other
problems.  I'm thinking we should use a different configuration relief.

If the RoHS solder does not fill the hole we would typically go back and
top solder the connection.  I know the industry considers this a no-no.

Any recommendations?

Thanks in advance.

Phil Nutting

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2