TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Carl Proescholdt <[log in to unmask]>
Date:
Tue, 2 Oct 2007 13:59:40 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (121 lines)
I wrote a small treatise on this earlier. Look in the archives. To
summarize; profile your new circuit boards with a new TC the first time
you set the board up.
For daily/weekly process control, make a fixture that clamps the TC
between two metal straps and measure the repeatability of the
temperature. You don't care what the actual temp is, just that it is the
same as yesterday (or last week). Expect your measurements do drop
slightly over time, and when it is out of the process window, time for
recalibration. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carl Proescholdt
Sent: Tuesday, October 02, 2007 1:43 PM
To: [log in to unmask]
Subject: Re: [TN] Thermocouple Longevity?

Also, consider where the same thermocouple technology is used in other
processes for precise control: Solder Pots, Multilayer presses, etc..
These are expected to be in service for years without changing.  

Carl
dca manufacturing

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Tuesday, October 02, 2007 1:37 PM
To: [log in to unmask]
Subject: Re: [TN] Thermocouple Longevity?

We are using the wire insulated with high temp cloth, Kevlar I believe. 
We have used them many times. The voltage / temperature values are
unchanged. 

This is a fundamental property of the materials. I would not expect to
see subtle drifting. 
If the weld is good and the connection at the plug is good, the wires
insulated one from the other up to the weld, the voltage measured at the
ends of the wire should be reliable and temperature dependent. 

I have seen failures of the insulation, cracks in the weld, and loose
connections inside the plug produce inaccurate measurements. 
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 02, 2007 2:04 PM
To: [log in to unmask]
Subject: [TN] Thermocouple Longevity?

Hi Everyone!
 
How many reflow profiles do ya'll put the same thermocouples through
before you think about replacing them?
 
I've typically used them until they quit working or the insulation
deteriorates so bad that I don't want to use them anymore. I was told
that was not a good practice. That your typical K thermocouple starts
drifting after only 4 or 5 thermal cycles. I said; "Really?" I didn't
want to debate a whole lot because it was a customer who said this, so I
just agreed and went on.
 
So, do any of you know this to be a fact, and do any of you trash a
thermocouple after only 4 or 5 profiles and replace them with new ones?
 
Kind regards,
 
Steve Gregory

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2