TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, ekalgren <[log in to unmask]>
Date:
Mon, 29 Oct 2007 09:21:11 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Louis Guérin <[log in to unmask]>
Subject:
From:
Louis Guérin <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (113 lines)
Eric,

Your assumption is good. As for the replacement, the MIL-S-13949H NOTICE 2 dated on 30 November 1998, which supersede the MIL-P-13949G, has the following on it;

MIL-S-13949H, dated 31 March 1993, is hereby canceled without replacement.

The IPC-4101A with Amendment1 replaces well the old MIL spec. It also has a reference to the MIL spec for a given specification sheet.

Hope will help.

Louis Guérin, C.I.D.+

Conception de Plaquette de Circuit Imprimé | PCB Designer

Lyrtech inc. 
Phone/ Tél.: (1) (418) 877-4644 #2242

Toll Free/Sans frais -  Canada &  USA : (1) (888) 922-4644 #2242
Fax /Téléc.: (1) (418) 877-7710 
www.lyrtech.com

Infinite possibilities...TM

-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de ekalgren
Envoyé : 26 octobre 2007 15:03
À : [log in to unmask]
Objet : [TN] PCB Material Question

This one should be easy enough for Friday.

 

I've got a drawing calling out the following material:

 

GE062 C2/C2 1A per MIL-P-13949

 

I've worked it out so far to be Type GE 0.0620 thick (they left out a 0),
with 2 oz copper on each side.

 

I can't figure out the 1A.  I think it should be A1 for pits/dents class A,
and class 1 for thickness tolerance.

 

Does this sound right?  Also, has anything replaced Mil-P-13949?  Is type GE
material commonly available?

 

Thanks!

 

Eric Kalgren

Electrical Engineer

Cobham Defense Electronic Systems 
Continental Microwave Division 
11 Continental Drive 
Exeter, NH  03833  USA
Tel:  603-775-5200  
Fax: 603-775-5201 
E-mail:[log in to unmask]  
Website:   <http://www.cobhamdes.com/> http://www.cobhamdes.com

 <mailto:[log in to unmask]>  

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

THIS MESSAGE AND ALL ATTACHED DOCUMENTS ARE EXCLUSIVELY INTENDED
TO THE INDICATED RECIPIENTS AND ITS CONTENTS MAY BE CONFIDENTIAL.
IT IS STRICTLY FORBIDDEN TO ANYONE TO TAKE COGNIZANCE, USE, OR
DIVULGE THE INFORMATION CONTAINED HEREIN. IF YOU MISTAKENLY
RECEIVE THIS MESSAGE, IMMEDIATELY INFORM LYRTECH AND DESTROY THE
MESSAGE AND ATTACHMENTS FORTHWITH.THANK YOU.

LE PRESENT MESSAGE ET LES DOCUMENTS QUI Y SONT JOINTS S'ADRESSENT
EXCLUSIVEMENT AU(X)DESTINATAIRE(S) INDIQUE(S) ET LEUR TENEUR PEUT
ETRE CONFIDENTIELLE. IL EST STRICTEMENT INTERDIT A QUICONQUE D'EN
PRENDRE CONNAISSANCE, DE LES UTILISER OU DE LES DIVULGUER. SI
VOUS RECEVEZ LE PRESENT MESSAGE PAR ERREUR, VEUILLEZ EN AVISER
LYRTECH IMMEDIATEMENT ET DETRUIRE LE MESSAGE SEANCE TENANTE,
AINSI QUE LES DOCUMENTS QUI Y SONT JOINTS.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2